Powder |
PPPC No. |
Typical Composition (wt.%) |
Particle Size (microns) |
Melting Point (ºC) |
Hardness | Function & Application |
Mo Agglomerated and sintered, spherical |
PR4210 | Mo:99.0+ |
-104~+44 -88~+44 -74~+38 -44 |
2610 | HRA:60~65 | Self-bonding with most metals and alloys, high bond strength with ceramics and glasses, resistant to gripping, wear and eroding of melting metals. Used as bond coatings, casting die coatings, piston ring and synchronizing disc coatings. |
Mo Sintered |
PR4211 | Mo:99.0+ |
-104~+44 -88~+44 -74~+38 -44 |
2610 | HRA:60~65 | Self-bonding with most metals and alloys, high bond strength with ceramics and glasses, resistant to gripping, wear and eroding of melting metals. Used as bond coatings, casting die coatings, piston ring and synchronizing disc coatings. |
Mo/25NiCrBSi Blended |
PR4231 |
Mo:75.0, NiCrBSi(HRC60):25.0 |
-104~+44 -88~+44 -74~+38 -44 |
1025(NiCrBSi) | HRC:40~45 | Dense and smooth, high bonding strength, excellent resistance to gripping and wear. Used as piston ring and synchronizing disc coatings. |
Mo/30NiCrBSi Blended |
PR4232 |
Mo:70.0, NiCrBSi(HRC60):30.0 |
-104~+44 -88~+44 -74~+38 -44 |
1025(NiCrBSi) | HRC:40~45 | Dense and smooth, high bonding strength, excellent resistance to gripping and wear. Used as piston ring and synchronizing disc coatings. |
Mo/70NiCrBSi Blended |
PR4233 |
Mo:30.0, NiCrBSi(HRC60):70.0 |
-104~+44 -88~+44 -74~+38 -44 |
1025(NiCrBSi) | HRC:50~55 | Dense and smooth, high bonding strength, excellent resistance to gripping and wear. Used as piston ring and synchronizing disc coatings. |
Mo-50Mo2C Agglomerated and sintered, spherical |
PR4221 | Mo:50.0, Mo2C:50.0 |
-104~+44 -88~+44 -74~+38 -44 |
2410 | HRA:60~65 | Self-bonding with most metals and alloys, high bond strength with ceramics and glasses, resistant to gripping, wear and eroding of melting metals. Used as bond coatings, casting die coatings, piston ring and synchronizing disc coatings. |
Mo-30Mo2C Agglomerated and sintered, spherical |
PR4222 | Mo:70.0, Mo2C:30.0 |
-104~+44 -88~+44 -74~+38 -44 |
2410 | HRA:60~65 | Self-bonding with most metals and alloys, high bond strength with ceramics and glasses, resistant to gripping, wear and eroding of melting metals. Used as bond coatings, casting die coatings, piston ring and synchronizing disc coatings. |
Mo/ 15Cr3C2/35NiCr Blended |
PR4271 | Mo:50.0, Cr3C2:15.0, NiCr:35.0 |
-104~+44 -88~+44 -74~+38 -44 |
1400(NiCr) | HRC:40~50 | Dense and smooth, high bonding strength, excellent resistance to gripping and wear. Used as piston ring and synchronizing disc coatings. |
Mo/ 10Cr3C2/40NiCr Blended |
PR4272 | Mo:50.0, Cr3C2:10.0, NiCr:40.0 |
-104~+44 -88~+44 -74~+38 -44 |
1400(NiCr) | HRC:40~50 | Dense and smooth, high bonding strength, excellent resistance to gripping and wear. Used as piston ring and synchronizing disc coatings. |
Mo/ 10Cr3C2/50NiCr Blended |
PR4273 | Mo:40.0, Cr3C2:10.0, NiCr:50.0 |
-104~+44 -88~+44 -74~+38 -44 |
1400(NiCr) | HRC:40~50 | Dense and smooth, high bonding strength, excellent resistance to gripping and wear. Used as piston ring and synchronizing disc coatings. |
Mo/ 20Cr3C2/50NiCr Blended |
PR4274 | Mo:30.0, Cr3C2:20.0, NiCr:50.0 |
-104~+44 -88~+44 -74~+38 -44 |
1400(NiCr) | HRC:40~50 | Dense and smooth, high bonding strength, excellent resistance to gripping and wear. Used as piston ring and synchronizing disc coatings. |
Mo/AlSi Blended |
PR4281 | Mo:50.0, AlSi:50.0 |
-104~+44 -88~+44 -74~+38 -44 |
650(AlSi) | HRA:40~50 | Excellent resistance to wear, gripping and scratching. Used as wear resistant coatings on sliding contact friction surfaces such as synchronizing discs and gear boxes. |